FAQ Can I use permeable resin jointing mortars with paving laid on an impermeable bed of mortar?

ruler

 

Introduction:

This is a commonly raised question: the paving is being laid on a (relatively) impermeable bed, so is it really OK to use a permeable jointing mortar? Won’t it cause problems? Won’t it lead to freeze/thaw failure?

Generally speaking, and for the vast majority of paving installations in Britain and Ireland, this really isn’t an issue.

 ribbon

The background:

When it comes to jointing, we now have over two decades of Europe-wide experience using good quality, two-component resin mortars with permeable, impermeable, or near-impermeable paving, whether that’s granite flagstones, porphyry cubes, basalt setts, concrete slabs, and so much more. These materials are, in some cases, laid onto a mortar, either a standard sand/cement mortar, a coarser grit/cement mortar or, more correctly, a highly permeable grit-based mortar.
resin mortar with porphyry setts
Resin mortar with porphyry setts
Most concretes and stones are slightly permeable – that’s why they look damp long after the rain has stopped. Porcelain and certain clay pavers are, to all intents and purposes, impermeable, so may require further consideration. However, the sand/cement mortar bedding most commonly used when laying paving is, more or less, impermeable*, yet we have countless examples of natural stone and other materials that have subsequently been jointed with a good-quality permeable two-part resin mortar and have continued to function without a problem.

* There is a growing trend to use highly permeable bedding mortars, but, for now, most installations are still laid on only-slightly-permeable mortars of one form or another.

It’s accepted that this absence of problems, particularly in Britain and Ireland, is due in no small part to the fact that we don’t get severe, prolonged, deep and hard frosts. Any frosts we get are relatively minor and short-lived, and rarely have the duration to adversely affect paving. This is why we are able to lay paving differently in Britain and Ireland, why we don’t need the deep frost-cover protection that we see in northern Europe, North America and elsewhere.

 ribbon

The Physics:

With most residential paving having a typical depth of 20-60mm, and joint widths of just 5-12mm, there is precious little jointing material to be affected by any sustained freeze. Any frost-induced expansion is so minimal, it exerts practically no pressure of significance onto the adjacent paving.
comparison between stone and resin mortar
Comparison between stone and resin mortar
Further, the compressive strength of the resin mortar is much lower than that of most stones so, if there was to be an exceptional frost, it would be the mortar that is "squeezed" and not the paving.
When water freezes solid, it expands by around 9%. This expansion is the cause of frost heave, the phenomenon that lifts paving from the ground and is thought, by some, to cause failure of permeable jointing products.

If a joint was 10mm wide and 20mm deep, filled entirely with water, we could expect a deep frost to create a ‘plug’ of ice that could be 10.9mm wide and 21.8mm deep at most.

However, such a joint is NOT completely filled with water. It’s mostly filled with aggregate and resin: the jointing material. For most two-part resin jointing mortars, a reasonable estimate would be that roughly 70% of the joint volume is fine aggregate and resin: only 30% can be water.

So, if we have only 30% water, the frost expansion can only be 30% of what it might be in a water-filled joint, so, instead of 10.9mm width, a frozen joint could only be a maximum of less than 10.3mm – just a third of a millimetre of expansion.

void space in jointing material
Joints have plenty of void space, even when filled
Further, when the edges are fully constrained, as is the case with most paving joints, the pressure exerted by a freeze will find the easiest outlet, and so any expansion is more likely to be upwards and out of the joint, and not sideways to exert pressure onto the paving.

Finally, bear in mind that, unlike cement-based mortars, most quality two-part resin mortars have a relatively high degree of elasticity. They are designed to be stretched and squeezed, and to recover without ill-effect. This elasticity of the mortar is relatively minimal, but it is more than enough to cope with the exertions of a British or Irish winter.

 ribbon

Water Penetration:

There are so many installations where quality two-part resin mortars have been used with paving having much wider and deeper joints, yet there are practically no jointing failures due to frost in Britain and Ireland. Setts may have joints that are 9-15mm in width and depths of 100mm or more, so considerably far more jointing material than patio paving, and therefore more potential for frost expansion, yet we just don’t see it. It doesn’t happen.

But what about water penetration? Surely that is detrimental to the performance and service life of a pavement, isn’t it?

carpet stones jointed
If, for argument’s sake, we regard the paving itself to be practically impermeable, and the bedding (the aforementioned sand/cement mortar) is similarly impermeable, there is only the volume of the joint available to act as a reservoir for any residual surface water – less the actual volume of the jointing mortar grains, of course.
If we further assume, again for argument’s sake, that 70% of the joint is filled with "solid" fine aggregate and resin, that leaves 30% void space which could, in theory, be filled with water. That’s the most that can be held. Try as we might, it’s impossible to get more water into that joint. Once the joint is filled with water (it’s known as ‘saturation’) no more water can enter. The impermeable bed and the impermeable paving won’t absorb any of the water (or will only absorb a negligible amount) so once the joint is saturated, no more water can enter. It’s full, and cannot, by definition, be fuller. saturated paving joint
Saturated paving joint
If, as stated above, no water (of any significant quantity) is able to penetrate the bed or the paving, then it cannot cause any significant damage. All that water can do is sit there, sulk a bit, and wait to be evaporated.
rainbow sandstone
Rainbow sandstone - probably more permeable than the mortar!
Now, there are permeable paving materials. In fact, there are some materials used for paving in Britain and Ireland that have a permeability which some believe could rival a bathroom sponge, Mint and Rainbow sandstone being just two of the worst offenders. In pavements where such materials have (inadvisably) been laid, we have to accept that moisture can enter the paving material.
But, even if we were to use a totally impermeable jointing material, say thiosulphite mastic or similar, moisture will still enter the paving via the surface, and when to compare the surface area of a flagstone to the area of edge in contact with jointing material, there’s far greater potential for that moisture to enter from the top, rather than the sides.

 ribbon

Think about our widespread use of granite, sandstone, limestone and all sorts of other natural paving materials that are, to greater or lesser extents, permeable. We wouldn’t consider rejecting these materials for pavement construction simply because they exhibit permeability.

In an ideal world, paving would be laid on a highly permeable bedding and jointed with a permeable material, so all that excess surface water could be directed to ground, as happen in an open field, rather than being channelled towards a man-made drainage system and dumped directly into our streams and rivers, or, even worse, sent for expensive and unnecessary cleaning at the local Effluent treatment Works.

For the less-than-ideal world in which we live, and given the highly variable installation methodologies which seems to be preferred in Britain, a permeable, quality, two-component resin mortar cannot damage quality paving. Poor quality paving might suffer, as might poor quality installation, but good quality paving properly installed has nothing to worry about from the use of a good quality two-part resin jointing mortar.